Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.60 kJ/m²
3.14 ft-lb/in²
ISO 180/1A
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Izod Impact, Notched (ISO) 6.60 kJ/m²
3.14 ft-lb/in²
ISO 180
LNP Lubricomp® LCL-4033 EM Polyetheretherketone, Carbon Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
Izod Impact, Notched (ISO) 6.60 kJ/m²
3.14 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
Izod Impact, Notched (ISO) 6.60 kJ/m²
3.14 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..