Izod Impact, Notched (ISO) 0.800 - 8.80 kJ/m²
0.381 - 4.19 ft-lb/in²
Average value: 5.37 kJ/m² Grade Count:3
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..