Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 40.47 kJ/m² | 19.26 ft-lb/in² | ISO 180 |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |