Polymer Property : Izod Impact, Notched (ISO) = 5.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.50 - 10.5 kJ/m²

@Temperature -20.0 - -20.0 °C
3.57 - 5.00 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 8.82 kJ/m² Grade Count:4
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..