Polymer Property : Izod Impact, Notched (ISO) = 5.19 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.00 - 10.9 kJ/m²
2.38 - 5.19 ft-lb/in²
Average value: 8.52 kJ/m² Grade Count:4
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..