Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.90 kJ/m²
3.28 ft-lb/in²
ISO 180/1A
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..