Izod Impact, Notched (ISO) 2.00 - 62.0 kJ/m²
0.952 - 29.5 ft-lb/in²
Average value: 11.4 kJ/m² Grade Count:8
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..