Polymer Property : Izod Impact, Notched (ISO) = 69.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 69.0 kJ/m²
32.8 ft-lb/in²
ISO 180-1A
Gromax BTE70-DN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.