Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 14.8 kJ/m²
7.04 ft-lb/in²
ISO 180
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..