Polymer Property : Izod Impact, Notched (ISO) = 7.21 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.70 - 7.21 kJ/m²
2.71 - 3.43 ft-lb/in²
Average value: 6.60 kJ/m² Grade Count:10
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..