Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.0 - 15.5 kJ/m² | 6.66 - 7.38 ft-lb/in² | ASTM D256 |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |