Polymer Property : Izod Impact, Notched (ISO) = 7.49 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.00 - 15.7 kJ/m²
1.90 - 7.49 ft-lb/in²
Average value: 6.94 kJ/m² Grade Count:67
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..