Polymer Property : Izod Impact, Notched (ISO) = 7.98 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.98 kJ/m²
3.80 ft-lb/in²
ISO 180/1A
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications..