Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 19.6 kJ/m²
9.33 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Pr..
Izod Impact, Notched (ISO) >= 19.6 kJ/m²
>= 9.33 ft-lb/in²
Sibur ABS 1106 Extrusion Grade ABS Plastic
With high deformation properties and sanitary-hygienic properties for production of sheets with following pneumatic and vacuum forming of internal parts of refrigerators, as well as for compounding ..
Izod Impact, Notched (ISO) >= 19.6 kJ/m²
>= 9.33 ft-lb/in²
Sibur ABS 1106M Extrusion Grade ABS Plastic
With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose.
Izod Impact, Notched (ISO) >= 19.6 kJ/m²
>= 9.33 ft-lb/in²
Sibur ABS 1530 Molding Grade ABS Plastic
Thermal resistance with higher fluidity for large and thin wall articles.