Polymer Property : Izod Impact, Notched (ISO) = 95.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
Izod Impact, Notched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific)
Blow moldable, impact modifed XENOY
Izod Impact, Notched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a..
Izod Impact, Notched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
Izod Impact, Notched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
ASTM D256
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry)
Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c..
Izod Impact, Notched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East)
Blow moldable, impact modifed XENOY