Izod Impact, Notched (ISO) 23.0 - 97.0 kJ/m²

@Temperature -50.0 - -50.0 °C
10.9 - 46.2 ft-lb/in²

@Temperature -58.0 - -58.0 °F
Average value: 44.5 kJ/m² Grade Count:8
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..