Polymer Property : Four Ball Extreme Pressure, Weld Load = 244.6 kg Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 244.6 kg
539.3 lb (mass)
Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE
Polyol Ester grease especially for high speed bearingsFeatures: Lubricating bearings operating under a wide range of conditions, including high speeds, extreme temperatures and high loads. Handles ..