Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.560 mm | 0.0220 in | |
ChevronTexaco FM Seamer Oil FeaturesChevron Seamer Oil FM is a premium performance industrial lubricant designed specifically to be used in Angelus Sanitary Can Machine Company seaming equipment and other similar applications... |