Mechanical Properties Metric English Comments
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips SUPER-STA NLGI No. 1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips SUPER-STA NLGI No. 2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Four Ball Wear 0.420 mm

@Temperature 75.0 °C,
Time 3600 sec
0.0165 in

@Temperature 167 °F,
Time 1.00 hour
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350/5
Chesterton 630 SXCF Synthetic, Extreme Pressure & Corrosion Resistant Grease
Description: Superior resistance to washout by water, caustics, sanitizing cleaners, process fluids and steam has now been combined with high temperature performance to product Chesterton® 630 SXCF..
Four Ball Wear 0.420 mm
0.0165 in
ChevronTexaco FM ISO 68 Lubricating Oil
Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr..
Four Ball Wear 0.420 mm
0.0165 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM 4172
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Four Ball Wear 0.420 mm
0.0165 in
Scar Diameter; ASTM D-2266
ConocoPhillips Grade 2 Calcium S Grease NLGI
Description: Conoco Calcium S Grease is a light, specialty calcium stearate thickened product that is used in the automotive assembly industry. It is amber in color and is used in applications where..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips Hydroclear® 15 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips Hydroclear® 150 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips Hydroclear® 460 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips SUPER-STA M NLGI No.0
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips SUPER-STA M NLGI No.2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Four Ball Wear 0.420 mm
0.0165 in
ChevronTexaco Black Pearl® NLGI 0 Grease EP
FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito..
Four Ball Wear 0.420 mm
0.0165 in
ChevronTexaco Black Pearl® NLGI 1 Grease EP
FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito..
Four Ball Wear 0.420 mm
0.0165 in
ChevronTexaco Black Pearl® NLGI 2 Grease EP
FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips Hydroclear® 68 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Wear 0.420 mm
0.0165 in
Scar Diameter; ASTM D-2266
ConocoPhillips Grade 1 Calcium M Grease NLGI
Description: Conoco Calcium M Grease is a specialty product that incorporates high load-carrying and antiwear capabilities with excellent low temperature properties and high-temperature stability af..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips Hydroclear® 320 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Wear 0.420 mm
0.0165 in
ConocoPhillips SUPER-STA M NLGI No.1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...