Polymer Property : Izod Impact, Notched (ISO) = 10.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 22.5 kJ/m²

@Temperature 23.0 °C
10.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Polyram PlusTek PA7800G33 Nylon 6.6 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Impact Modified
33% Glass fiber reinforced, heat stabilized, impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram.