Polymer Property : Izod Impact, Notched (ISO) = 14.7 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 14.7 kJ/m²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Izod Impact, Notched (ISO) 14.7 kJ/m²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct..
Izod Impact, Notched (ISO) 14.7 kJ/m²

@Temperature -30.0 °C
7.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..