Izod Impact, Notched (ISO) 35.7 kJ/m²

@Temperature -40.0 °C
17.0 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy
Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago