Polymer Property : Izod Impact, Notched (ISO) = 17.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 36.0 kJ/m²

@Temperature 23.0 °C
17.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Izod Impact, Notched (ISO) 36.0 kJ/m²

@Temperature 23.0 °C
17.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Terluran® SP-6 ABS
Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Izod Impact, Notched (ISO) 36.0 kJ/m²

@Temperature -20.0 °C
17.1 ft-lb/in²

@Temperature -4.00 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6  (Unverified Data**)
Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an..