Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.62 kJ/m²

@Temperature -17.8 °C
2.20 ft-lb/in²

@Temperature 0.000 °F
ISO 180/1A
ExxonMobil AP3N Polypropylene Impact Copolymer
Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos..
Izod Impact, Notched (ISO) 4.62 kJ/m²

@Temperature -17.8 °C
2.20 ft-lb/in²

@Temperature 0.000 °F
ISO 180/1A
ExxonMobil PP7684KN Impact Copolymer
Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance ..