Polymer Property : Izod Impact, Notched (ISO) = 24.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East)
CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
11.4 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 80
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free
Information Provided by LG Chem
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
11.4 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Ineos ABS Lustran® 288 ABS, Injection Molding Grade
Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 180-1A
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Ineos ABS Lustran® ABS 640 Injection Molding Grade
Lustran® ABS 640 has high impact strength and is injection molding grade.
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Hostacomâ„¢ CB271FC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB271FC high melt flow, 2,400 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Novodur® H701 ABS
Novodur H701 is an injection molding grade of ABS with heat resistance and high impact strength.Information provided by Styrolution
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -40.0 °C
11.4 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4; ISO 180/1A
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded
BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned
Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, Conditioned
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
Izod Impact, Notched (ISO) 24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..