Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.41 kJ/m²

@Temperature -17.8 °C
2.10 ft-lb/in²

@Temperature 0.000 °F
ISO 180/1A
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..