Polymer Property : Izod Impact, Notched (ISO) = 4.98 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.98 kJ/m²

@Temperature -40.0 °C
2.37 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
S&E Specialty Polymers TufFill™ 5701 Black PP
Application: High Calcium carbonate filed, high heat resistance thermoplastic extrusion grade based on polypropylene copolymer/homopolymer.Information provided by S&E Specialty Polymers