Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h..
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X6800BM PBT
Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**)
Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NB50 NL IT PA 6 super tough
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..