Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
63.5*12.7*3.2; ISO 180/4A
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Europe-Africa-Middle East)
Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI)..
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Izod Impact, Notched (ISO) 78.0 kJ/m²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
63.5*12.7*3.2; ISO 180/4A
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific)
Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI)..