Polymer Property : Izod Impact, Notched (ISO) = 83.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry)
Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o..