Polymer Property : Izod Impact, Notched (ISO) = 9.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 18.9 kJ/m²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Izod Impact, Notched (ISO) 18.9 kJ/m²

@Temperature 22.8 °C
9.00 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..