Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.20 MPa @Thickness 2.00 mm |
1040 psi @Thickness 0.0787 in |
Flow Injection molded; ISO 37 |
PolyOne OnFlex™ S HS 70A-3E2543 Thermoplastic Elastomer (TPE) This OnFlex™-S HS thermoplastic elastomer compounds is based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver high strength and medium-low density in add.. |