Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 114 MPa @Temperature 23.0 °C |
16500 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |