Tensile Strength at Break >= 128 MPa

@Temperature 150 °C
>= 18600 psi

@Temperature 302 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength at Break 128 MPa

@Temperature 23.0 °C
18600 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I..