Mechanical Properties Metric English Comments
Tensile Strength at Break 947 MPa

@Temperature 700 °C
137000 psi

@Temperature 1290 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium ..