Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 14.5 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.100 MPa

@Temperature 107 °C
14.5 psi

@Temperature 225 °F
T-Block on Aluminum; ASTM D987
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Tensile Strength at Break 0.100 MPa

@Temperature 150 °C
14.5 psi

@Temperature 302 °F
T-Block on Aluminum; ASTM D987
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Tensile Strength at Break 0.100 MPa

@Temperature 107 °C
14.5 psi

@Temperature 225 °F
T-Block on Aluminum; ASTM D987
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Tensile Strength at Break 0.100 MPa

@Temperature 150 °C
14.5 psi

@Temperature 302 °F
T-Block on Aluminum; ASTM D987
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Copyright © lookpolymers.com All Rights Reserved