Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 1490 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.3 MPa

@Temperature 23.0 °C
1490 psi

@Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® G3548L TPC-ET  (Unverified Data**)
Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec..