Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1034 MPa @Temperature 538 °C |
150000 psi @Temperature 1000 °F |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |