Mechanical Properties Metric English Comments
Tensile Strength at Break 1300 MPa

@Temperature 50.0 °C
189000 psi

@Temperature 122 °F
Special Metals UDIMET® alloy 520 Superalloy
UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris..