Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 19.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.8 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2870 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type 1, 200 mm/min; Flow; DIN 53504
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Strength at Break 19.8 MPa

@Temperature 100 °C,
Time 259000 sec
2870 psi

@Temperature 212 °F,
Time 72.0 hour
Circulating Oven Aging
LG Chemical NBR 6850 High Acrylonitrile Polymer
Description: NBR 6850 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6850 is a non staining, medium mooney, an..