Polymer Property : Tensile Strength at Break = 193 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 193 MPa

@Temperature 23.0 °C
28000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Strength at Break 193 MPa

@Temperature 23.0 °C
28000 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..