Tensile Strength at Break 22.4 MPa

@Treatment Temp. 100 °C,
Time 259000 sec
3250 psi

@Treatment Temp. 212 °F,
Time 72.0 hour
Aged ASTM D #3 Oil
LG Chemical NBR 3280 High Acrylonitrile Polymer
Description: NBR 3280 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3280 is a non staining, high..