Tensile Strength at Break 23.0 MPa

@Temperature 90.0 °C
3340 psi

@Temperature 194 °F
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced
ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Strength at Break 23.0 MPa

@Temperature 120 °C
3340 psi

@Temperature 248 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..