Polymer Property : Tensile Strength at Break = 27.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa

@Temperature 145 °C,
Time 2990 sec
3920 psi

@Temperature 293 °F,
Time 0.830 hour
cured; ASTM D412
LG Chemical NBR 6230 High Acrylonitrile Polymer
Description: NBR 6230 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6230 is a non staining, low mooney, and m..
Tensile Strength at Break 27.0 MPa

@Temperature 150 °C
3920 psi

@Temperature 302 °F
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer
Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..