Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1900 MPa @Temperature 300 °C |
276000 psi @Temperature 572 °F |
R<sub>m</sub> |
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |