Polymer Property : Tensile Strength at Break = 38.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.6 MPa

@Temperature 23.0 °C
5600 psi

@Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..