Polymer Property : Tensile Strength at Break = 4000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.6 MPa

@Thickness 0.0254 mm
4000 psi

@Thickness 0.00100 in
Transverse to Flow; ASTM D882
Diamond Polymers NPP11-0119 Linear Low Density Polyethylene with Antiblock
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.