Polymer Property : Tensile Strength at Break = 4290 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.6 MPa

@Thickness 0.0200 mm
4290 psi

@Thickness 0.000787 in
Direction of Flow; ASTM D882
Diamond Polymers NPP11-0218 Linear Low Density Polyethylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.