Tensile Strength at Break >= 380 MPa

@Temperature 20.0 °C
>= 55100 psi

@Temperature 68.0 °F
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p..