Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 43.0 MPa @Temperature 150 °C |
6240 psi @Temperature 302 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 43.0 MPa @Temperature 23.0 °C |
6240 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |